A patented coating eliminates the chance of an angioplasty balloon being punctured or damaged during stent delivery and post-stent dilation.

A patented coating eliminates the chance of an angioplasty balloon being punctured or damaged during stent delivery and post-stent dilation. It increases the coefficient of friction between stent and balloon surface so there is no movement or slippage. The coating can be produced from a variety of polymers. Balloons can be produced in a range of sizes, configurations, lengths, and burst pressures. Wall thickness is typically 5 to 50 µ. Balloons are available with 0.5 to 50-mm diameters and sizes from 2 to 12 mm.
Advanced Polymers Inc., 13 Industrial Way, Salem, NH 03079, (603) 898-8962.

Sponsored Recommendations

NEW Low Profile, Ultra Compact Power Supplies

March 13, 2024
Learn more HERE about Altech's Power supplies!

Altech's Liquid Tight Strain Relifs Catalog

March 13, 2024
With experienced Product Engineers and Customer Service personnel, Altech provides solutions to your most pressing application challenges. All with one thought in mind - to ensure...

Industrial Straight-Through Cable Gland

March 13, 2024
Learn more about Altech's cable glands and all they have to offer for your needs!

All-In-One DC-UPS Power Solutions

March 13, 2024
Introducing the All-In-One DC-UPS, a versatile solution combining multiple functionalities in a single device. Serving as a power supply, battery charger, battery care module,...

Voice your opinion!

To join the conversation, and become an exclusive member of Machine Design, create an account today!